Hastelloy and Inconel are two well-known families of nickel-based alloys used in demanding industrial environments. Both offer excellent corrosion resistance, high-temperature performance, and mechanical strength, but they are designed for different service requirements.
So, what is the difference between Hastelloy and Inconel?
Generally, Hastelloy alloys prioritize resistance to aggressive chemical environments, while Inconel alloys are widely recognized for high strength, oxidation resistance, and elevated-temperature performance. This guide compares their composition, properties, applications, pricing, and welding characteristics to help you select the right alloy.
Hastelloy is a family of nickel-based corrosion-resistant alloys developed for demanding chemical and industrial environments. These alloys typically contain varying amounts of chromium, molybdenum, iron, and other alloying elements to resist corrosion, pitting, crevice corrosion, and stress corrosion cracking.
Different Hastelloy grades are designed for specific service conditions. For example:
Hastelloy C-276: Offers broad resistance to various aggressive chemicals, including oxidizing and reducing environments.
Hastelloy C-22: Provides excellent resistance to pitting, crevice corrosion, and localized corrosion in mixed chemical environments.
Hastelloy B-2: Particularly suitable for handling hydrochloric acid and other reducing environments.
Hastelloy X: A nickel-chromium-iron-molybdenum alloy designed primarily for high-temperature strength and oxidation resistance.
Hastelloy alloys are commonly used in chemical processing equipment, reactors, heat exchangers, pollution control systems, and other equipment exposed to corrosive media.
Inconel is a family of nickel-based alloys known for high strength, oxidation resistance, and reliable performance at elevated temperatures.
Depending on the grade, Inconel alloys may contain chromium, iron, molybdenum, niobium, titanium, and aluminum. Some grades are strengthened through solid-solution strengthening, while others achieve high strength through precipitation hardening.
Common Inconel grades include:
Inconel 600: A nickel-chromium alloy offering good oxidation and corrosion resistance at elevated temperatures.
Inconel 625: A nickel-chromium-molybdenum-niobium alloy with excellent corrosion resistance and high strength without requiring precipitation hardening.
Inconel 718: A precipitation-hardenable nickel-iron-chromium alloy offering exceptionally high tensile strength, fatigue resistance, and creep resistance.
Inconel X-750: A precipitation-hardenable alloy used in high-temperature springs, fasteners, and other demanding components.
Inconel alloys are widely used in aerospace, gas turbines, power generation, oil and gas, and high-temperature industrial equipment.
Yes. Both Hastelloy and Inconel belong to the nickel-based alloy family and offer corrosion resistance, high-temperature performance, and good mechanical properties.
However, they are not interchangeable. Hastelloy generally emphasizes resistance to aggressive chemical corrosion, while many Inconel grades are designed for high-temperature strength and oxidation resistance. Their actual performance depends on the individual grade.
Ronsco supplies Hastelloy and Inconel nickel alloy materials, as well as nickel alloy TIG and MIG welding wires. Whether you need plates, sheets, bars, pipes, or welding consumables, contact us with your requirements to request product details and a quotation.
Contact Us for a QuoteChemical composition is one of the main differences between Hastelloy and Inconel. Both contain nickel as a major alloying element, but their chromium, molybdenum, iron, niobium, and other element contents vary considerably.
The following table compares four representative grades. Values are in weight percentage (%).
| Element | Hastelloy C-276 | Hastelloy C-22 | Inconel 625 | Inconel 718 |
|---|---|---|---|---|
| Nickel (Ni) | Balance | Balance | ≥58.0 | 50.0–55.0 |
| Chromium (Cr) | 14.5–16.5 | 20.0–22.5 | 20.0–23.0 | 17.0–21.0 |
| Molybdenum (Mo) | 15.0–17.0 | 12.5–14.5 | 8.0–10.0 | 2.8–3.3 |
| Iron (Fe) | 4.0–7.0 | 2.0–6.0 | ≤5.0 | Balance |
| Tungsten (W) | 3.0–4.5 | 2.5–3.5 | — | — |
| Niobium + Tantalum (Nb+Ta) | — | — | 3.15–4.15 | 4.75–5.50 |
| Titanium (Ti) | — | — | — | 0.65–1.15 |
| Aluminum (Al) | — | — | — | 0.20–0.80 |
Note: These are representative compositional ranges and limits, not guaranteed values for every supplied product. Actual requirements should be verified against the applicable ASTM, ASME, AMS, or manufacturer specifications.
Hastelloy C-276, C-22, and Inconel 625 are nickel-based alloys with significant chromium and molybdenum additions. Inconel 718 contains more iron and uses precipitation-hardening elements to achieve high mechanical strength.
Chromium contributes to oxidation and corrosion resistance by forming a protective oxide layer. Inconel 625 and Hastelloy C-22 typically contain higher chromium levels than Hastelloy C-276, although corrosion performance cannot be determined by chromium content alone.
Molybdenum improves resistance to localized corrosion, particularly pitting and crevice corrosion. Hastelloy C-276 and C-22 contain considerably more molybdenum than Inconel 718, making them suitable for many aggressive chemical environments.
Tungsten contributes to the corrosion-resistant characteristics of Hastelloy C-276 and C-22. Inconel 718 contains niobium, titanium, and aluminum, which help form strengthening precipitates during heat treatment.
Although both alloy families perform well under demanding conditions, their individual grades have different strengths.
Corrosion resistance is one of the most important differences between Hastelloy and Inconel.
Hastelloy C-276 and C-22 are particularly suitable for aggressive chemical environments. Their chromium and molybdenum contents help resist pitting, crevice corrosion, and stress corrosion cracking.
Inconel alloys also offer excellent corrosion resistance, but performance varies by grade:
Inconel 625: Provides excellent resistance to seawater, chloride-containing environments, and various industrial chemicals.
Inconel 600: Offers good resistance to oxidation and several corrosive environments at elevated temperatures.
Inconel 718: Provides good corrosion resistance alongside high mechanical strength, but is not designed to replace C-276 or C-22 in every aggressive chemical environment.
Which is better for corrosion resistance?
For many highly aggressive chemical processing environments, Hastelloy C-276 and C-22 are often preferred. However, Inconel 625 can also provide excellent corrosion resistance in marine, offshore, and chemical processing applications.
The correct selection depends on the chemical medium, concentration, temperature, and operating conditions.
Both alloy families include grades suitable for high-temperature applications, but their performance characteristics differ.
Inconel is widely recognized for high-temperature strength and oxidation resistance. Inconel 600 is commonly used in elevated-temperature environments, while Inconel 718 offers excellent strength, creep resistance, and fatigue performance at high temperatures.
Hastelloy also includes high-temperature grades. For example, Hastelloy X is designed for oxidation resistance and mechanical stability in high-temperature environments.
However, corrosion-resistant grades such as C-276 and C-22 are generally selected primarily for corrosion performance rather than maximum high-temperature strength.
Mechanical strength varies significantly between individual grades.
Inconel 718 is particularly well known for its high tensile and yield strength, achieved through precipitation hardening. It is widely used in aerospace components, turbine parts, and other applications requiring high strength under demanding conditions.
Hastelloy C-276 and C-22 also provide good mechanical strength, but their primary design focus is corrosion resistance rather than achieving the highest possible tensile strength.
Inconel alloys, particularly nickel-chromium grades, are widely used in environments involving high temperatures and oxidizing gases. Hastelloy X also offers excellent oxidation resistance and is suitable for furnace components, industrial heating equipment, and gas turbine applications.
The best choice depends on the temperature range, atmosphere, and required service life.
Hastelloy and Inconel serve different industrial requirements, although their application areas sometimes overlap.
Hastelloy is commonly selected for equipment exposed to aggressive chemicals and corrosive operating conditions.
Typical applications include:
Chemical processing reactors and vessels
Heat exchangers and pressure vessels
Pharmaceutical manufacturing equipment
Flue gas desulfurization systems
Acid production and handling equipment
Pollution control equipment
Offshore and marine chemical processing systems
Common grades include C-276, C-22, B-2, and X.
Inconel alloys are widely used in applications requiring high strength, oxidation resistance, and reliable performance under elevated temperatures.
Typical applications include:
Aerospace engines and turbine components
Gas turbines and power generation equipment
Oil and gas exploration equipment
Heat treatment furnaces
Nuclear power systems
Marine engineering
High-temperature fasteners and structural components
Common grades include Inconel 600, 625, 718, and X-750.
| Application | Commonly Selected Alloy | Reason |
|---|---|---|
| Chemical reactors | Hastelloy C-276 | Resistance to aggressive chemical environments |
| Acid processing equipment | Hastelloy C-276 / B-2 | Corrosion resistance in suitable acid environments |
| Marine equipment | Inconel 625 | Excellent resistance to seawater and chloride environments |
| Aerospace turbine components | Inconel 718 | High strength and fatigue resistance |
| High-temperature furnaces | Inconel 600 / Hastelloy X | Oxidation resistance and high-temperature performance |
| Chemical heat exchangers | Hastelloy C-22 / Inconel 625 | Corrosion resistance under application-specific conditions |
The price of Hastelloy and Inconel varies depending on the alloy grade, product form, dimensions, manufacturing process, and market conditions.
There is no fixed rule that Hastelloy is always more expensive than Inconel, or vice versa.
Certain Hastelloy grades, such as C-276 and C-22, can carry higher prices due to their alloying element content, specialized manufacturing requirements, and corrosion-resistant applications.
However, some Inconel grades, particularly Inconel 718, can also be relatively expensive because of their complex alloy composition, precipitation-hardening requirements, and demanding production specifications.
A meaningful price comparison should therefore be made between specific grades and equivalent product forms.
Several factors influence the final purchasing price:
Chemical composition: Nickel, molybdenum, chromium, niobium, and other alloying elements affect raw material costs.
Material grade: Different grades require different alloying and manufacturing processes.
Product form: Plates, sheets, bars, rods, pipes, tubes, and welding wires may have different production costs.
Dimensions and specifications: Thickness, diameter, tolerances, and technical requirements influence processing costs.
Order quantity: Larger orders may offer more competitive unit pricing.
Market conditions: Nickel and other alloying element prices fluctuate over time.
For accurate pricing, buyers should provide the required grade, product form, dimensions, quantity, and applicable standards when requesting a quotation.
Both Hastelloy and Inconel can be welded using appropriate welding processes and filler metals. TIG (GTAW) welding is commonly used for nickel-based alloys because it provides good control over heat input and weld quality.
Filler metal selection depends on the specific alloy grade, joint design, welding procedure, and service requirements.
Yes. Hastelloy alloys can be welded using suitable processes, including TIG (GTAW), MIG (GMAW), and other qualified welding methods.
Proper filler metal selection and welding procedures are essential to maintain corrosion resistance and mechanical properties. For corrosion-resistant Hastelloy grades, matching or appropriately overalloyed filler metals are commonly used.
The appropriate TIG welding wire depends on the specific Hastelloy grade.
Common filler metal classifications include:
| Base Metal | Common TIG Filler Wire |
|---|---|
| Hastelloy C-276 | ERNiCrMo-4 |
| Hastelloy C-22 | ERNiCrMo-10 |
| Hastelloy B-2 | ERNiMo-7 |
| Hastelloy C-4 | ERNiCrMo-7 |
| Hastelloy B-3 | ERNiMo-10 |
For example, ERNiCrMo-4 is commonly used for welding Hastelloy C-276, while ERNiCrMo-10 is used for Hastelloy C-22.
The final filler metal selection should follow the applicable welding procedure specification (WPS), base metal requirements, and intended service environment.
Inconel alloys also require appropriate nickel-based filler metals.
Common TIG welding wire classifications include:
| Base Metal | Common TIG Filler Wire |
|---|---|
| Inconel 600 | ERNiCr-3 |
| Inconel 625 | ERNiCrMo-3 |
| Inconel 718 | ERNiFeCr-2 |
| Inconel X-750 | Application-specific filler metal selection |
For example, ERNiCrMo-3 is widely used for welding Inconel 625, while ERNiFeCr-2 is commonly used for Inconel 718.
For dissimilar metal joints or special operating conditions, the filler metal selection may differ from the standard matching classification.
Choosing between Hastelloy and Inconel should be based on the actual operating environment rather than simply comparing their general material properties.
The equipment is exposed to highly aggressive chemical environments.
Resistance to pitting and crevice corrosion is a major requirement.
The application involves strong acids or mixed chemical media.
Long-term corrosion resistance is more important than maximum mechanical strength.
High tensile strength and fatigue resistance are essential.
The equipment operates under elevated temperatures.
Oxidation resistance is a key requirement.
The application involves aerospace, turbines, power generation, or demanding structural components.
Certain grades overlap in their capabilities. Inconel 625, for example, offers excellent corrosion resistance, while Hastelloy X provides strong high-temperature performance.
Ultimately, the right material should be selected according to the specific chemical environment, operating temperature, mechanical loading, and relevant industry standards.
Hastelloy is a registered trademark used for a family of nickel-based alloys. It does not have one universal alternative name.
Individual Hastelloy grades are also identified by their UNS designations. For example, Hastelloy C-276 is UNS N10276, while Hastelloy C-22 is UNS N06022.
When purchasing materials, buyers should confirm both the commercial grade name and the corresponding UNS designation.
Not necessarily. Although both are nickel-based alloys, their chemical compositions and corrosion characteristics differ.
Replacing one with the other requires evaluating the operating environment, mechanical requirements, applicable standards, and material compatibility. A direct substitution should not be made without engineering approval.
Some Inconel grades, particularly Inconel 718, offer higher tensile and yield strength than many commonly used corrosion-resistant Hastelloy grades.
However, strength varies by grade and heat treatment condition. It is not accurate to say that every Inconel alloy is stronger than every Hastelloy alloy.
Hastelloy C-276 and C-22 are often preferred for highly aggressive chemical environments. However, Inconel 625 also provides excellent corrosion resistance in many marine and chemical processing applications.
The final choice depends on the corrosive medium, concentration, temperature, and exposure conditions.
Not always. Prices depend on the specific grade, alloy composition, product form, manufacturing requirements, and market conditions. A grade-to-grade quotation is the most reliable way to compare costs.
Ronsco supplies nickel alloy materials and nickel alloy welding consumables for industrial applications. We offer a range of alloy grades, product forms, and specifications to meet different customer requirements.
Whether you need Hastelloy or Inconel materials, or nickel alloy TIG and MIG welding wires, Ronsco is committed to providing reliable products and consistent supply support.
Contact Ronsco today to discuss your material requirements and request a quotation.
Ronsco is a trusted global supplier of nickel alloy and stainless steel welding wires, including Inconel, Hastelloy, and Monel series. Our products are manufactured to meet industry standards and are widely used in demanding applications such as aerospace, oil & gas, chemical processing, and power generation. Explore our resource center for the latest industry insights, product knowledge, and technical references.
Contact us for a quote or technical assistance.